Cushion Pads
Sector
Building machinery
Application
Cushion Pads
Solution
Cushion pads made of TECAST
Description
When ramming concrete piles of varying lengths into the subsurface, cushion pads are used to absorb the impact energy.
Requirement profile
- High energy absorption
- Good recovery elasticity
- Balanced ratio of strength to toughness
Material chosen
TECAST mod. offers the ideal combination of toughness and strength for differing soil conditions – allowing the cushions to withstand long operating periods.
Physical Properties
Property | Standard | Value | Unit | |
|---|---|---|---|---|
Density | DIN 53 479 | 1,14 | g/cm³ | |
Water Absorption (23°C, 50% r.h.) | ISO 62 | 2,8 | % | |
Mechanical |
|
| ||
Tensile Strenght at Yield | DIN EN ISO 527 | 60/45* | MPa | |
Elongation at Break | DIN EN ISO 527 | >100 | % | |
Tensile Modulus | DIN EN ISO 527 | >1800 | MPa | |
Thermal | ||||
Coefficient of Thermal Expansion | DIN 53 752 | 8 - 9 | 10-5/K | |
Melting point | ISO-R 75 (A) | 214 | °C | |
*moist |